• 2011 aluminum plate
    • 2011 aluminum plate
    Alloy 2011 is known as a free machining alloy or 'FMA' - this means that the material has excellent machinability and is suitable for use on automatic lathes. The alloy displays poor corrosion resistance and therefore anodising will be required for additional surface protection. Whilst weldability...
    • 2014 aluminum plate
    • 2014 aluminum plate
    Grade 2014A is a high strength aluminium alloy which retains its strength after heat treatment. It is a 4 - 5% copper alloy and is supplied in the fully heat-treated condition (solution heat treated & artificially aged). The material offers very good machinability and is used widely in the...
    • 2024 aluminum plate
    • 2024 aluminum plate
    Alloy 2024 is one of the more prominent aluminium alloys. Due to the alloys good fatigue resistance, especially in thick plate form, the material is specified for use in the aerospace and military sector in fuselage applications in such areas as structures and wing tension members. With improved...
    • 2124 aluminum plate
    • 2124 aluminum plate
    Aluminium Alloy for use in Moderately Elevated Temperatures 2124 Aluminium Alloy is a higher purity form of 2024 and was developed specifically for elevated temperature applications. The aerospace sector is a primary market for this alloy as fracture toughness of the material is guaranteed, and can...
    • 2219 aluminum plate
    • 2219 aluminum plate
    2219 Aluminium is a high strength alloy used in high temperature structural applications including space boosters and fuel tanks. The alloy benefits from good mechanical properties combined with good machinability. With good fracture toughness the alloy is useful over a temperature range of -452°...
    • 2618a aluminum plate
    • 2618a aluminum plate
    2618A - a strong aluminium alloy containing nominally 2% copper and 1.5% magnesium. The alloy is produced as bar, plate, tube and is also available as clad sheet and strip. Solution treated and artificially aged to achieve the T6 condition or with the addition of controlled stretching to achieve...